The Absorption Test

This is usually called the water absorption test. This is a simple test conducted on all stones. It consists of keeping a cubical specimen of the stone of about 50 g weight immersed in water for 24 hours and finding the volume of the absorbed water. This is represented as a percentage of absorption by weight. This percentage should not be more than 0.6%. This test is also called the electrical resistance test.